Megatron Modifier

Hardening accelerator, waterproofing additive


Appointment:

   Super- accelerator, waterproofing additive to concrete

Features:

  • Concrete solutions and waterproofing properties acquired;

  • Acceleration time setting;

  • Plasticity (solution does not „sit“);

  • Increased adhesion;

  • Significantly reduces subsidence solution.

  • Can be used as an accelerator and waterproof with different mixes (plaster, adhesives, solutions, concretes)

Recommendations for use:

Waterproof plaster

   For application of waterproof cement - sand plaster on a wet surface of concrete or masonry - old plaster slips, surface cleaned, rinsed with water, mounted net. Modifier closing in clean water. At one modifier of ten parts water and mix thoroughly. Then preparing a dry mixture of 1 part cement (not below grade M-400) and 2 parts of dry sand. The resulting mixture is cooked to shut the solution and mix thoroughly. The solution is to apply a layer of 3 - 5 cm. Before that, if necessary, perform tamping places much filtered water.

Cracks tamponage

   Before the tamponage crack must be cleaned of weak particles using jackhammers, chisels or metal brush, rinsed with water. Modifier is added to a clean water. Add 1 part of modifier per 6 parts of water and mix thoroughly. The dry mix is ​​prepared from Portland cement and dry sand in a ratio of 1: 1 by volume. The resulting dry mixture to shut prepared solution and thoroughly mixed for 1.5 - 2 minutes to obtain a thick plastic mass. From the fact that the solution is grasped quickly (about 5 minutes) - kneading it should be in small quantities. The resulting solution tightly fills cracks and smoothes down. In the case of very strong pressure leak, the water leaching solution - until setting - use materials waterproofing systems TM Megatron Megatron Seal.

Floor Waterproofing

   For waterproofing screed mixture prepared from 1 part of cement and 2 parts of sand mixed with the solution of the modifier in a ratio of 1 part of modifier  to 10 parts of water. Thickness contraction is from 3 to 5 cm. From raising the wall it is 10 - 12 cm. For swimming it is the entire height of the cup. After processing tanks with drinking water it needs 2-3 times to change the water.

Concrete

   Concrete is kneaded in small quantities because it is quickly grasped. Start time setting concrete solution depends on the proportion of modifier and takes about 5 minutes.

Appointment

Dry mix

The solution concentrate with water

Hardening time

Waterproofing plaster

1 part cement

2 parts sand

1 part concentrate

10-20 parts water

from 10-30

Under water tamponage

1 part cement

2 parts sand

1 part concentrate

3 parts water

2-3

For tamponage joints and cracks

1 part cement

2 parts sand

1 part concentrate

10 parts water

from 5-15

For concreting in water and

waterproofing

1 part cement

2 parts sand

1 part concentrate

10 parts water

from 10-30

 

Scope:

  • When laying concrete directly into the water

  • To divert water;

  • To repair structures under water;

  • To speed up the stucco with a big thick coating

Safety:

    Work performed in protective glasses and rubber gloves. The substance contains alkali, in contact with skin or eyes rinse with plenty of water and seek medical advice.
    Complies with State Standard 24211-91 Additives for concrete, DBN V.2.7-64-97 Terms of use of chemical additives in concrete and mortar, water-repellent Technical Conditions  6-02-700 group.

Characteristic Value Conformity ДСТУ

1

Appearance

Transparent liquid

ДСТУ Б В.2.7-171:2008

2

Basic

Aluminate

ДСТУ Б В.2.7-171:2008

3

Density g / cm3

1,05-1,07

ДСТУ Б В.2.7-171:2008

4

The acidity of pH

10

ДСТУ Б В.2.7-171:2008

5

Shelf life

12

ДСТУ Б В.2.7-171:2008